| Term / international symbol | Verifiable standard | Key parameter | Acceptance reading in this market | Anchored entity |
|---|---|---|---|---|
| Anti-fingerprint (AFP) finish AFP · anti-fingerprint | YB/T 4333-2013T/ZZB 2549-2021GB/T 9286-2021 | H2O contact angle ≥ 105° · oleic acid ≥ 75° · ≥ 5 000 rub cycles · cross-cut grade 0 · pencil ≥ 2H | Acceptance rests on contact angle and rub cycles; adhesion is graded by cross-cut, not by a hand-wipe impression. | P9 · C / Adhesion · Pencil hardness · AFP coating |
| Stainless honeycomb panel Honeycomb panel | GB 8624GB/T 3280-2015 | core 5–20 mm · face 0.3–3.0 mm · large-format panel, no stiffener | Flatness of large panels comes from the core, not a thicker face; the reaction-to-fire class needs a test report rather than a verbal 'non-combustible' claim. | P9 · A / Substrate & Dimensions · 12-series honeycomb delta |
| PVD vacuum ion plating PVD · vacuum ion plating | GB/T 18705GB/T 10125-2021 | film 0.8–1.2 μm · phase TiN / TiCN / CrN / ZrN · NSS ≥ 500 h (GB/T 10125-2021) | Colour names are not acceptance criteria; film phase, thickness and salt-spray result are. A sealed reference is still required across batches of the same colour code. | P9 · B/C / Film phase · Film thickness · NSS |
| Elevator stainless cladding Elevator cladding · PT A | T/CEA 0024-2021GB/T 7588.1-2020GB/T 3280-2015 | PREN ≥ 15.0 · PT A tolerance ±0.02 mm · t ≥ 1.5 mm | On large car-wall panels, thickness tolerance affects visual flatness more than the grade does; coastal projects additionally require a pitting-resistance check. | P9 · A / Thickness tolerance · Grade |
| Colour deviation & batch control ΔE*ab · colour deviation | GB/T 7921ASTM D2244ISO/CIE 11664-4 | ΔE*ab ≤ 1.0 (GB/T 7921) · sealed reference · multi-point instrument reading | Colour difference is judged by instrument readings against a sealed reference at several points; 'looks the same' is not an acceptance result. Same-furnace colouring must be written into the contract. | P9 · B / Colour deviation · TERM ΔE*ab |
| Neutral salt spray & coastal corrosion NSS · neutral salt spray | GB/T 10125-2021ISO 9227ASTM B117 | ≥ 240 h (GB/T 10125-2021) · 316L + PVD ≥ 500 h · 5 % NaCl · 35 ± 2 °C | Salt-spray hours are meaningful only when the test standard, substrate and coating combination are stated; re-testing is required after weld passivation. | P9 · C / Neutral salt spray |
| Export conformity & lift directive CE · UKCA · 2014/33/EU | 2014/33/EUEN 81-20/50GB/T 26572 | notified-body type examination · factory production control audit · UKCA for GB market | The destination market's approval scheme, with its applicable edition and year, must be stated in the contract. Only verifiable designations are listed here; national codes are not invented. | P9 · S-map / EN · ISO cross-reference |
| Antibacterial surface Antibacterial · ISO 22196 | ISO 22196 | CNAS-accredited lab report required · no numeric claim published without evidence | Antibacterial efficacy requires a report from a qualified third-party laboratory; without one, no figure is published and no performance is promised. | P9 · C / Durability & Compliance (report-gated) |
| Low-carbon & recycled steel RoHS · A1 · recycled steel | GB/T 265722011/65/EU(EU) 2015/863GB 8624 | A1 reaction to fire (GB 8624) · RoHS 2011/65/EU · recycled content stated per contract | Environmental conclusions rest on test reports and declarations of conformity; recycled content and carbon-footprint figures are agreed separately in the contract and are not published on the page. | P9 · C / Reaction to fire · RoHS conformity |
| Surface finish codes 2B · HL · No.4 · 8K · ET · EMB | GB/T 3280-2015GB/T 1031GB/T 9754 | 2B Ra ≤ 0.5 μm · 8K Ra ≤ 0.02 μm (GB/T 1031) · 60° GU ≥ 800 (GB/T 9754) | 8K and No.8 name the same mirror surface in different systems; acceptance rests on measured Ra and 60° gloss, not on the trade code. | P9 · B / Finish code · Roughness Ra · Gloss 60° |
| Water-ripple & honeycomb embossed ceiling panels Water-ripple / honeycomb embossed ceiling panel | GB/T 3280-2015GB 8624ASTM A480GB/T 1031 | t 0.6–0.8 mm · 1500 × 3000 mm · mechanically formed relief (no printed layer) · flatness per GB/T 3280-2015 · reaction-to-fire class per GB 8624 | Ceilings are viewed from a distance, so gauge serves stiffness rather than impact resistance. The relief is mechanically formed, with no printed layer to fade or peel. Acoustic control comes from perforation and backing, fixed at quotation stage because it changes material take-off and cost per square metre. The reaction-to-fire class requires a test report. | P9 · A / Substrate & Dimensions · Embossed relief |
| Artificial weathering & UV durability Artificial weathering · xenon-arc UV | GB/T 1865GB/T 16422.2ISO 16474-2GB/T 7921 | xenon-arc exposure (GB/T 1865) · colour shift judged by ΔE*ab per GB/T 7921 · gloss retention per GB/T 9754 · no numeric exposure claim without a test report | Outdoor durability cannot rest on a verbal promise: light source, irradiance and cycle conditions must be stated. Post-ageing colour shift and gloss retention are judged instrumentally; exposure hours not confirmed in a test report are not published. | P9 · C / Durability & Compliance · Weathering |
| Substrate grade & mill test certificate 304 / 316L · EN 10204 3.1 MTC | ASTM A240EN 10204 3.1GB/T 20878 | Cr / Ni / Mo content and tensile properties per ASTM A240 · grade designation per GB/T 20878 · heat-number traceability via EN 10204 3.1 MTC · no numeric claim without a mill certificate | Grade is established by the mill certificate and heat number, never inferred from colour or finish. For coastal work the pitting-resistance index is calculated from the certified chemistry, and spectrometric verification is logged at acceptance. | P9 · A / Grade · Substrate chemistry · Heat-number traceability |
| Intergranular corrosion & weld sensitisation IGC · intergranular corrosion / weld sensitisation | GB/T 4334-2020ASTM A262ISO 3651-2 | method E (Cu-CuSO4-H2SO4, boiling) per GB/T 4334-2020 · 180° bend, no intergranular cracks on outer surface · ASTM A262 Practice A/E · ISO 3651-2 · low-carbon or stabilised grade for welded parts | Welded fabrications are not cleared by grade alone. After the boiling copper-sulphate test the specimen is bent; acceptance requires no intergranular cracks on the outer bend surface. Mandrel diameter and bend angle belong in the test commission. | P9 · C / Durability & Compliance · Weld sensitisation |
| Cyclic corrosion testing (intermittent salt spray & humidity cycling) CCT · cyclic corrosion test (intermittent salt spray + humidity cycling) | GB/T 20853-2026ISO 16701:2025GB/T 10125-2021ISO 9227 | programme A (constant dew point) / programme B (constant temperature) per GB/T 20853-2026 (IDT ISO 16701:2025) · intermittent salt-solution spray + humidity cycling · relative corrosion ranking only; the standard sets neither exposure duration nor acceptance threshold · contrast with continuous NSS per GB/T 10125-2021 / ISO 9227 | A cyclic test ranks relative resistance under chloride contamination and humidity cycling; it is not a service-life forecast. State which programme is commissioned, constant dew point or constant temperature, together with the salt solution and cycle conditions. The standard sets neither exposure duration nor acceptance criteria; those belong to the product specification. Cycle counts cannot be converted directly into hours of continuous neutral salt spray. Austenitic grades may show excessive pitting under this method, so results are read against the real service environment. | P9 · C / Durability & Compliance · Cyclic corrosion (CCT) |
| Pitting & crevice corrosion testing / CPT Pitting / crevice corrosion · CPT / CCT | GB/T 17897-2026ASTM G48-25 | method A (GB/T 17897-2026): 6 % FeCl3, 22 ± 1 °C / 50 ± 1 °C, 72 h, corrosion rate in g/(m²·h) by mass loss · method B (GB/T 17897-2026): potentiostatic critical pitting temperature (CPT) · ASTM G48-25 methods A–F (CPT / CCT) · relative grade ranking only, not a service-life prediction | A pitting-resistance index calculated from chemistry is a screening value, not an acceptance result. When commissioning coastal work, state whether the ferric-chloride immersion method or the potentiostatic critical-temperature method is used, and fix solution concentration and temperature. Outcomes rank grades relative to one another and must not be converted into years of service; surface condition, welds and passivation shift the result, so fix them in the test commission. | P9 · A/C / PREN · Coastal pitting · Grade chemistry verification |
| Verifiable standard | Test object / scope |
|---|---|
| GB/T 17897-2026 | pitting corrosion test for stainless steels: ferric-chloride immersion (chemical) and potentiostatic critical pitting temperature (electrochemical); in force since 2026-11-01, replaces GB/T 17897-2016 |
| ASTM G48-25 | pitting and crevice corrosion resistance in ferric chloride solution, methods A-F including critical pitting / crevice temperature |
| GB/T 20853-2026 | accelerated cyclic corrosion test, intermittent salt-solution spray and humidity cycling (IDT ISO 16701:2025) |
| ISO 16701:2025 | artificial-atmosphere cyclic corrosion test under controlled humidity cycling and intermittent salt spray |
| GB/T 4334-2020 | intergranular corrosion test, methods A / B / C / E / F / G |
| ASTM A262 | detecting susceptibility to intergranular attack in austenitic stainless steels |
| ISO 3651-2 | resistance to intergranular corrosion, ferritic / austenitic / duplex steels and weldments |
| YB/T 4333-2013 | anti-fingerprint coating |
| T/ZZB 2549-2021 | anti-fingerprint performance |
| GB/T 9286-2021 | cross-cut adhesion |
| GB 8624 | reaction to fire |
| GB/T 3280-2015 | cold-rolled sheet, tolerance |
| GB/T 18705 | PVD decorative coating |
| T/CEA 0024-2021 | lift stainless cladding |
| GB/T 7588.1-2020 | lift safety, car walls |
| GB/T 7921 | colour difference CIE Lab |
| ASTM D2244 | instrumental colour difference |
| ISO/CIE 11664-4 | CIE Lab colour difference |
| GB/T 10125-2021 | neutral salt spray |
| ISO 9227 | corrosion tests in artificial atmospheres |
| ASTM B117 | salt spray apparatus |
| 2014/33/EU | lift directive |
| EN 81-20/50 | lift design and examination |
| ISO 22196 | antibacterial activity on plastics / surfaces |
| GB/T 26572 | RoHS restricted substances |
| 2011/65/EU | RoHS directive |
| (EU) 2015/863 | RoHS phthalates amendment |
| GB/T 1031 | surface roughness parameters |
| GB/T 9754 | gloss at 60° |
| ASTM A480 | finish designations |
| GB/T 20878 | stainless steel grades |
| GB/T 1865 | artificial weathering, filtered xenon-arc radiation |
| GB/T 16422.2 | laboratory light exposure, xenon-arc |
| ISO 16474-2 | coatings exposure to filtered xenon-arc |
| ASTM A240 | Cr / Ni / Mo chemistry and tensile properties of stainless plate, sheet and strip |
| EN 10204 3.1 | metallic products, inspection document type 3.1 (mill test certificate) |