DZMT · 鼎钻钢业
SPECIFICATION INTELLIGENCE / P9 · 2026-11-22
Specification Intelligence
DZMT · SPECIFICATION INTELLIGENCE / P9

Specification Intelligence

PARAMETERS · UNITS · STANDARDS · EIGHT LANGUAGES
Answer firstSpecification data is not a translation exercise. Every parameter is resolved into seven columns — symbol, SI typical value, imperial conversion, tolerance, governing standard, international cross-reference and selection rule. Symbols, figures, units and drawings stay identical across languages; only prose is written natively. 8K in Chinese, No.8 in English and 8K 鏡面 in Japanese therefore denote the same Ra ≤ 0.02 μm surface, and no knowledge of Chinese is needed to specify it.
Editorial basisValues on this page are typical specifications / nominal design ranges under the cited test standards, not batch-measured results. Measured values are governed by the test report. Unverified figures on project counts, capacity, lead time and minimum order quantities are not published.
To keep numerals and units from being reordered inside RTL scripts such as Arabic, every value and symbol is isolated with bdi and locked to LTR. Imperial conversions are computed from ISO 80000 factors as a reading aid; contracts and test reports remain SI-only.
01

Grouped specification matrix · 24 rows

A · Substrate & Dimensions

ParameterSymbolTypical value (SI)ImperialTolerance / rangeStandard · cross-referenceSelection rule
Substrate gradeGrade304 / 316L / 201 / 430GB/T 20878AISI 304 / 316L / 201 / 430per melt analysisGB/T 20878ASTM A240 · EN 10088-2 · JIS G4305 · ISO 15510C1–C2 → 304 / 201 · C3 → 304 · C4–C5 → 316L
Thicknesst0.3–3.0 mmGB/T 32800.012 in – 0.118 in±0.02–0.10 mmGB/T 3280ASTM A480 · EN 10088-2 · JIS G4305 · ISO 9445t ≥ 1.0 mm → 8K / EMB · t ≤ 1.0 mm → HL / SB
Standard sheet sizeW × L1219 × 2438 / 1219 × 3048 mmGB/T 328048 × 96 / 48 × 120 in+0 / −2 mm (nominal)GB/T 3280ASTM A480 · EN 10088-2 · JIS G4305W ≤ 1219 mm → stock · W > 1219 mm → made to order
Maximum sheet sizeW × L max1500 × 6000 mmGB/T 328059.06 in × 236.22 inflatness ≤ 1.0 mm/mGB/T 3280ASTM A480 · EN 10088-2L > 3048 mm → honeycomb backing recommended
Thickness toleranceΔt±0.02–0.10 mmGB/T 3280±0.0008 in – 0.0039 inby gauge classGB/T 3280ASTM A480 · ISO 9445 · EN 10088-2mirror / large format → tighter half-tolerance
Density & mass per areaρ / m·A⁻¹7.93 g/cm³ · 1.0 mm ≈ 7.93 kg/m²GB/T 208780.2865 lb/in³ · 1.0 mm ≈ 1.62 lb/ft²304 / 304L nominal densityGB/T 20878ASTM A240 · EN 10088-2 · ISO 15510m/A ∝ t · honeycomb ≈ 1/3 of solid (published)

B · Surface & Optics

ParameterSymbolTypical value (SI)ImperialTolerance / rangeStandard · cross-referenceSelection rule
Finish codeFinish code2B / BA / No.4 / HL / 8K / No.8GB/T 32802B / BA / No.4 / No.8 (ASTM A480)mill finish → polishedGB/T 3280ASTM A480 · EN 10088-2 · JIS G43052B → base · No.4 → HL · 8K/No.8 → mirror
Roughness RaRa2B ≤ 0.5 μm · 8K ≤ 0.02 μmGB/T 10312B ≤ 19.7 μin · 8K ≤ 0.8 μincut-off 0.8 mm · ISO 4287GB/T 1031ASME B46.1 · EN ISO 4287 · JIS B0601 · ISO 21920Ra ↓ → specularity ↑ · handle with AFP
Gloss 60°GU (60°)8K ≥ 800 GU · No.4 120–220 GUGB/T 9754same instrument geometry 60°glossmeter 60° / ISO 2813GB/T 9754ASTM D523 · EN ISO 2813 · JIS Z8741 · ISO 2813GU ≥ 800 → low-touch interior only
Colour deviationΔE*ab≤ 1.0 (same lot) / ≤ 1.5 (lot-to-lot)GB/T 7921CIE Lab · D65 / 10° · instrument readingvs. sealed sampleGB/T 7921ASTM D2244 · EN ISO 11664-4 · JIS Z8730 · ISO/CIE 11664-4ΔE → sealed sample + multi-point measurement
PVD film thicknesst_PVD0.8–1.2 μmGB/T 187050.031 mil – 0.047 mil±0.15 μmGB/T 18705ISO 1463 · ASTM B487 · EN ISO 1463t_PVD ↑ → colour depth ↑ · check adhesion
Film phaseFilm phaseTiN · TiCN · CrN · ZrNGB/T 18705TiN / TiCN / CrN / ZrN (phase notation)reactive PVD · Ar + N₂ / C₂H₂GB/T 18705ISO 1463 · ASTM B487TiN → gold · CrN → gunmetal · ZrN → brass

C · Durability & Compliance

ParameterSymbolTypical value (SI)ImperialTolerance / rangeStandard · cross-referenceSelection rule
Neutral salt sprayNSS≥ 240 h · 316L + PVD ≥ 500 h (no red rust)GB/T 10125-20215 % NaCl · 35 ± 2 °C · continuous sprayISO 9227 NSSGB/T 10125-2021ASTM B117 · EN ISO 9227 · JIS Z2371 · ISO 9227C4–C5 → 316L + PVD + weld passivation
AdhesionAdhesionCross-cut grade 0GB/T 9286-2021ASTM D3359 5B equivalent1 mm grid · 6 × 6 cutsGB/T 9286-2021ASTM D3359 · EN ISO 2409 · JIS K5600-5-6 · ISO 2409all coated systems · after pretreatment
UV ageingQUV≥ 500 h · no marked shift / chalkingGB/T 16422.3UVA-340 · 0.89 W/m² · 60 °C / 50 °C cycleISO 4892-3 cycle 1GB/T 16422.3ASTM G154 · EN ISO 4892-3 · JIS K7350-2 · ISO 4892-3exterior / high UV → re-check ΔE after QUV
Film hardnessHardness≥ 6 H (pencil) · film HV per reportGB/T 67396H pencil · Wolff-Wilborn / ISO 15184750 g loadGB/T 6739ASTM D3363 · EN ISO 15184 · JIS K5600-5-4 · ISO 15184high-touch → ≥ 6H + AFP
Reaction to fireReaction to fireA1 (non-combustible substrate)GB 8624metal substrate · no organic binder in coreclassification per systemGB 8624EN 13501-1 A1 · ASTM E136 · ISO 1182A1 applies to metal skin · composite core assessed separately
RoHS conformityRoHSConformity to 2011/65/EU · (EU) 2015/863GB/T 2657210 restricted substances · IEC 62321 test routedeclaration + test reportGB/T 26572IEC 62321 · EN 50581 / EN IEC 63000export / public projects → declaration dossier

D · Fabrication & Delivery

ParameterSymbolTypical value (SI)ImperialTolerance / rangeStandard · cross-referenceSelection rule
Fabrication processesProcessShear / bend / punch / laser / TIG / roll / etch / PVDGB/T 3280same process chain · symbol notationprotective film retainedGB/T 3280ASTM A480 · EN 10088-2finish last · protect face during fabrication
Minimum bend radiusR_minR ≥ 1 t (304, annealed, transverse)GB/T 232R / t ≥ 1 · bend axis ⊥ rolling directionper ISO 7438GB/T 232ASTM E290 · EN ISO 7438 · JIS Z2248 · ISO 7438mirror / embossed → R ≥ 2 t · trial bend first
WeldingWeldTIG / MIG · post-weld pickling & passivationGB/T 985.1ER308L / ER316L filler · Ar shieldingheat tint removedGB/T 985.1ISO 9692-1 · AWS A5.9 · EN ISO 14343C4–C5 → passivation mandatory · re-check NSS
Surface protectionAFPNano anti-fingerprint coat (optional)GB/T 9286-2021AFP · transparent · gloss shift ≤ 5 GUapplied after colouringGB/T 9286-2021ISO 2409 · ASTM D3359 · IEC 62321high-touch → AFP · re-check adhesion
Sampling & sealed sampleSamplingSealed sample + multi-point per pieceGB/T 7921reference sample retained for lot comparisonD65 / 10° · 60° geometryGB/T 7921ASTM D2244 · ISO/CIE 11664-4 · ISO 2813ΔE / GU judged vs. sealed sample, not eyesight alone
Mill test certificateMTCMTC 3.1 / test report / certificateGB/T 3280EN 10204 3.1 equivalent · heat-number traceabilityper delivery lotGB/T 3280EN 10204 3.1 · ASTM A480 · ISO 10474traceability → heat No. ↔ MTC ↔ delivery lot
02

Technical drawings · language-neutral

FIG. 01 / SHEET & GAUGEW = 1219 mm / 48 inL = 2438 mm3048 mm96 / 120 inSECTION tt = 0.3 - 3.0 mmDt = +/- 0.02 - 0.100.0118 - 0.1181 inMAX 1500 x 6000 mm59.06 x 236.22 in
Fig. 1 · Sheet and gauge: W × L is nominal size, t nominal thickness, Δt the thickness tolerance band.
FIG. 02 / FILM STACK ( um )304 / 316L SUBSTRATE0.3 - 3.0 mmPRETREATMENT (DEGREASE / ACTIVATE)—PVD TiN / TiCN / CrN / ZrN0.8 - 1.2 umAFP NANO-COAT (OPTIONAL)—00.40.81.21.62.0umCOLOUR = FILM STRUCTURE / NOT PAINT
Fig. 2 · Film stack: substrate → pretreatment → PVD film → anti-fingerprint layer; scale in μm, symbols shared across languages.
FIG. 03 / FINISH LADDER vs Ra ( um )2B0.50umNo.40.20um8K0.05um10K0.03um12K0.02umRa DECREASING -> SPECULARITY INCREASING ( SCHEMATIC )
Fig. 3 · Finish ladder and roughness scale: 2B → No.4 → 8K → 10K → 12K, with Ra decreasing stepwise (schematic, not to scale).
FIG. 04 / TOLERANCE BANDUPPER +0.08 mm / +0.0031 inLOWER -0.08 mm / -0.0031 inNOMINAL 0.00t ( NOMINAL )ACCEPTANCE = SI TOLERANCE IN CONTRACT / TEST REPORTISO 80000 / GB/T 3280 / ISO 9445
Fig. 4 · Reading a tolerance band: nominal value centred, upper and lower deviations on either side; SI tolerances govern contracts and test reports.
03

Industry symbols explained · 16 entries

2B

Cold-rolled, annealed and pickled matte mill finish; the common starting point for hairline, mirror, etching and PVD.

GB/T 20878
No.4 / HL

A unidirectional continuous abrasive grain, typically 240–600 grit; keep the grain direction consistent across adjoining panels.

GB/T 3280
8K / No.8

A high-reflectance mirror produced by multi-stage polishing; called 8K in China and No.8 in ASTM A480 — the same Ra ≤ 0.02 μm surface.

GB/T 3280
10K / 12K

Higher polish grades beyond 8K; trade designations rather than standard classes. Acceptance rests on measured Ra and 60° gloss, not the label.

GB/T 3280
Ra

Arithmetical mean roughness of the profile, in μm; lower values mean a smoother, more specular surface. State cut-off and evaluation length.

GB/T 1031
GU (60°)

Gloss reading at 60° geometry, dimensionless; 8K typically ≥ 800 GU, No.4 about 120–220 GU. Compare only under the same instrument geometry.

GB/T 9754
ΔE*ab

Total colour difference in CIE Lab space, dimensionless; measured against a sealed reference sample at several points per piece, by instrument rather than eyesight.

GB/T 7921
NSS

Neutral salt spray, 5 % NaCl at 35 ± 2 °C continuous fog, reported in hours; a comparative corrosion test for coating systems, not a service-life prediction.

GB/T 10125-2021
QUV

Laboratory accelerated UV ageing, typically UVA-340 lamps with condensation cycles; used to observe colour shift and chalking, read together with a ΔE re-check.

GB/T 16422.3
PVD

Physical vapour deposition: target atoms are sputtered in a vacuum and form TiN / TiCN / CrN / ZrN compound films on the substrate. Colour comes from film structure, not paint.

GB/T 18705
TiN / TiCN / CrN / ZrN

Common PVD phases: TiN gold, TiCN rose/gunmetal, CrN silver-grey, ZrN brass. Hue follows reactive gas ratio and bias; the sealed sample governs.

GB/T 18705
AFP

A transparent nano anti-fingerprint coating that reduces oil adhesion. It shifts gloss slightly, so it is applied after colouring and followed by adhesion and gloss re-checks.

GB/T 9286-2021
A1

Non-combustible class. The metal skin itself is A1; a honeycomb panel with an organic core or adhesive must be classified as a complete system, not by the skin alone.

GB 8624
MTC 3.1

An EN 10204 3.1 mill test certificate, signed by the manufacturer's authorised representative, carrying heat number and measured chemistry / mechanical values — the traceability chain sheet → heat → report.

GB/T 3280
C1 – C5

Atmospheric-corrosivity classes after ISO 12944-2: C1 dry indoor, C2 standard interior, C3 humid / public touch, C4 coastal / waterside, C5 high-salt exterior. Grade and protection escalate with the class.

GB/T 10125-2021
R / t

Ratio of minimum bend radius to thickness. For annealed 304 with the bend axis transverse to rolling, R ≥ 1 t; mirror or embossed faces call for R ≥ 2 t and a trial bend.

GB/T 232
04

Cross-border standard map · 14 sets

IDTest objectGB / ChinaASTM / USEN / EuropeJIS / JapanISO / International
S01Grade & chemistryGB/T 20878ASTM A240 / A959EN 10088-2JIS G4305ISO 15510
S02Sheet size & toleranceGB/T 3280ASTM A480/A240EN 10088-2JIS G4305ISO 9445
S03Surface roughnessGB/T 1031ASME B46.1EN ISO 4287JIS B0601ISO 4287 / 21920
S04Gloss 60°GB/T 9754ASTM D523EN ISO 2813JIS Z8741ISO 2813
S05Colour difference CIE LabGB/T 7921ASTM D2244EN ISO 11664-4JIS Z8730ISO/CIE 11664-4
S06Neutral salt sprayGB/T 10125-2021ASTM B117EN ISO 9227JIS Z2371ISO 9227
S07Cross-cut adhesionGB/T 9286-2021ASTM D3359EN ISO 2409JIS K5600-5-6ISO 2409
S08UV ageing QUVGB/T 16422.3ASTM G154EN ISO 4892-3JIS K7350-2ISO 4892-3
S09Pencil hardnessGB/T 6739ASTM D3363EN ISO 15184JIS K5600-5-4ISO 15184
S10Reaction to fire A1GB 8624ASTM E136EN 13501-1JIS A1321ISO 1182
S11RoHS restricted substancesGB/T 26572—EN 50581 / IEC 62321JIS C0950IEC 62321
S12Bend testGB/T 232ASTM E290EN ISO 7438JIS Z2248ISO 7438
S13Mill test certificateGB/T 3280ASTM A480EN 10204 3.1JIS G0415ISO 10474
S14Decorative welded tubeGB/T 18705ASTM A554EN 10296-2JIS G3446ISO 1127
National adoption noteRussia, India, Bangladesh and Gulf markets generally adopt the ISO series as national standards by identical endorsement. Only verifiable GB / ASTM / EN / JIS / ISO designations are listed here; state the adopted edition and year in the purchase contract and test commission. Unverified national designations are not invented.
05

Selection tree · C1 → C5

ClassExposureGradeFinishProtectionVerification
C1DRY INDOOR304 / 2012B / HL / 8K / ETAFP optionalGB/T 7921 · GB/T 9754
C2STANDARD INTERIOR304HL / SB / VR / EMBAFP optionalGB/T 7921 · GB/T 1031
C3HUMID / PUBLIC TOUCH304 / 316LHL / SB + AFPAFP + passivationGB/T 10125-2021 · GB/T 9286-2021
C4COASTAL / NEAR WATER316LPVD + AFPPVD + AFP + weld passivationGB/T 10125-2021 · GB/T 18705
C5HIGH SALT / EXTERIOR316LPVD + AFPPVD + AFP + sealed sample + mock-upGB/T 10125-2021 · GB/T 16422.3
Environment classes C1–C5 follow the atmospheric-corrosivity logic of ISO 12944-2. Grade, finish and protection are combined stepwise as a starting point only; the final choice rests on a site-specific exposure assessment and mock-up acceptance.
06

Dual-unit conversion factors

SI basisFactorImperial resultSI unit symbolImperial unit symbol
1 mm× 0.0393700787= 0.039370 inmmin
1 μm× 0.0393700787= 0.039370 milμmmil
1 μm× 39.3700787400= 39.370079 μinμmμin
1 kg/m²× 0.2048161436= 0.204816 lb/ft²kg/m²lb/ft²
1 g/cm³× 0.0361272920= 0.036127 lb/in³g/cm³lb/in³
07

Frequently asked questions

Are 2B, No.4 and 8K the same thing?
Not the same surface, but one shared grading language. 2B is the matte cold-rolled / annealed / pickled base; No.4 (HL) is a 240–600 grit unidirectional grain; 8K (No.8) is a multi-stage polished mirror. They are separated by Ra and 60° gloss — symbols and figures need no translation.
Is ΔE ≤ 1.0 (GB/T 7921) the same as 'no visible difference'?
No. ΔE*ab is an instrument reading in CIE Lab space, tied to D65/10° geometry, a sealed reference sample and multi-point sampling per piece. Visual judgement depends on illuminant and observer and cannot replace the reading; only ΔE is used here as the acceptance criterion.
Why 316L + PVD + post-weld passivation for coastal work?
Chlorides in C4–C5 exposure cause pitting and red rust. Mo in 316L raises pitting resistance, the PVD film adds a barrier, and post-weld pickling / passivation restores the chromium-depleted heat-affected zone. These are serial conditions; omitting any one requires an NSS re-check on the mock-up, under GB/T 10125-2021 and GB/T 18705.
Can GB/T be substituted for ASTM / EN / JIS / ISO?
Not substituted, but mapped. The same test object carries different designations, and specimen size, cycle parameters and interpretation rules may differ. Fourteen cross-reference sets are given here for search and communication; acceptance still follows the standard edition named in the contract. For Russian, Indian, Bangladeshi and Arabic-language markets, state the endorsed ISO edition and year in the contract.
08

Related pages

Back to collections