J05 · TECHNICAL ESSAY

Salt Spray, UV Ageing, Adhesion: Three Tests and How to Read Them

DZMT TECHNICAL EDITORIAL

Hours on a report mean nothing until a standard number is attached.

The answer first

A durability claim must be split into three non-interchangeable lines: corrosion (neutral salt spray, GB/T 10125-2021 / ASTM B117), light ageing (QUV, ASTM G154) and film adhesion (cross-cut, GB/T 9286-2021 / ASTM D3359). Each probes a different failure mode; none substitutes for another. Figures are typical values cited to standards, with measured values governed by the test report.

Typical values per test standard · measured values per test report

THE ARGUMENT

01 / 4

Salt spray: corrosion, not fading

Neutral salt spray probes resistance to pitting and red rust in a chloride environment, read per GB/T 10125-2021 (aligned with ASTM B117). Published typical figures place 304 with PVD at NSS ≥ 240 h and 316L with PVD at 500 h without red rust. Salt fog and UV ageing are not the same and cannot be converted into one another.

02 / 4

QUV: cycles of light and moisture

UV ageing combines fluorescent UV with condensation or spray cycles to observe colour shift, chalking and gloss loss, commonly read per ASTM G154. High-UV plateaus, large glazed roofs and exterior signage need this line; quoting salt-spray hours alone for an interior project answers the wrong question.

03 / 4

Cross-cut: is the film actually attached

The cross-cut test measures film-to-substrate adhesion per GB/T 9286-2021 (aligned with ASTM D3359 5B). For PVD, patinated and coated systems, adhesion governs peeling while salt spray governs rusting — two things routinely conflated.

04 / 4

Put all three in one table

A technical annex should list environment class, substrate grade, film system, salt-spray basis and duration, QUV basis and duration, adhesion grade, colour-deviation basis, and the clause that measured values follow the test report. Without the environment class, no number of hours can be judged sufficient.

TECHNICAL FACTS

TestFailure modeBasisTypical figureUse
Neutral salt spray (NSS)Pitting / red rustGB/T 10125-2021≥ 240 h;316L+PVD 500 hCoastal / waterside
UV ageing (QUV)Colour shift / chalkingASTM G154≥ 500 hExterior / high UV
Cross-cut adhesionPeeling / delaminationGB/T 9286-2021Grade 0All film systems
Film hardnessScratchingVickers methodPer reportHigh-touch surfaces
Thermal resistanceFilm structure changeThermal shockPer reportLuminaires / oven trim
Typical values per test standard · measured values per test report

Frequently asked

Do 500 salt-spray hours equal years outdoors?
No. There is no universal conversion between accelerated testing and service life; the environment class, maintenance cycle and project-specific review must be combined, with measured values governed by the test report.
Is QUV needed indoors?
Most conventional interiors can prioritise adhesion and colour deviation; strongly daylit atria and positions near UV sources should retain the ageing line.
Who issues the report and how?
A qualified laboratory issues it, stating the standard number, specimen description, conditions and results; the annex should cite the report number rather than copy an isolated figure.