Sea air does not read drawings; it only notices the molybdenum.
Failures in coastal and waterside projects are driven mainly by chloride pitting and crevice corrosion rather than uniform rust. Decide in order: classify atmospheric corrosivity at the site, then set the substrate (316L for high salt and humidity), then the finish and film combination, then testing and maintenance. The table below indexes selections by province-level region for scheme-stage orientation; the project assessment and test report govern.
Chloride ions breach the passive film locally, initiating pits in crevices, welds and beneath deposits. Molybdenum stabilises that film in chloride media, which is why 316L is repeatedly specified for coastal, pool and hot-spring work. De-icing salts and chloride cleaners carry the same risk into non-coastal northern cities.
Coastal is not one class: distance to shoreline, prevailing wind, elevation, shelter and maintenance access all alter actual salt deposition. The C1–C5 labels below are scheme-level indices flagging which regions need separate review; they do not replace a site-specific assessment.
High-salt work normally pairs a 316L substrate with a PVD film and an anti-fingerprint nano-coating; welds require passivation so they do not become preferential attack sites. Fasteners, backing plates and dissimilar-metal contacts must be reviewed for galvanic coupling, or the node fails before the panel does.
The table lists climate zone, corrosivity index, recommended grade and finish, and acceptance focus by province-level region. It serves scheme-stage orientation and long-tail retrieval; the final value in every row is governed by the project assessment, sealed sample and test report.
Coastal cladding and exterior elements need an agreed rinse cycle and inspection points, focusing on crevices, drainage paths and rear ventilation. Writing maintenance into the handover is more useful than debating the grade after rust appears; measured values follow the test report.
| Region | Climate zone | Corrosivity | Grade | Finish | Acceptance focus |
|---|---|---|---|---|---|
| Guangdong | South China coast | C4 high salt / humidity | 316L | PVD + AFP | GB/T 10125-2021; weld passivation |
| Guangxi | South China coast | C4 high salt / humidity | 316L | PVD + AFP | Separate grade assessment |
| Hainan | South China coast | C5 high salt / heat | 316L | PVD + AFP | Chloride pitting; typhoon fixings |
| Fujian | Southeast coast | C4 high salt / humidity | 316L | PVD + AFP | Salt spray; film adhesion |
| Zhejiang | East China coast | C3–C4 | 316L / 304 | PVD / HL | Plum-rain season; batch consistency |
| Shanghai | East China coast | C3–C4 | 316L / 304 | PVD / 8K | Cladding flatness; urban atmosphere |
| Jiangsu | East China coast | C3 | 304 | HL / SB | Large-format deflection; ΔE |
| Shandong | East China coast | C3–C4 | 316L / 304 | PVD / HL | Near-shore salt; de-icing salts |
| Hebei | North China coast | C3 | 304 | HL / EMB | Industrial fallout; cleaning cycle |
| Tianjin | North China coast | C3–C4 | 316L / 304 | PVD / HL | Coastal salt; port atmosphere |
| Liaoning | Northeast coast | C3 | 304 / 316L | HL / SB | Freeze–thaw; weld corrosion |
| Beijing | North China inland | C2 | 304 | 8K / ET | Interior colour deviation; AFP |
| Shanxi | North China inland | C2 | 304 | HL / EMB | Dry atmosphere; dust |
| Inner Mongolia | Northwest dry-cold | C1–C2 | 304 / 201 | SB / VR | Thermal range; dry shrinkage |
| Henan | Central China | C2–C3 | 304 | HL / PVD | Seasonal humidity; batch ΔE |
| Hubei | Central humid | C3 | 304 | PVD / AFP | Humid-heat ageing; QUV |
| Hunan | Central humid | C3 | 304 | HL / EMB | Plum-rain surface protection |
| Jiangxi | Central humid | C3 | 304 | PVD / SB | Humidity; acid rain |
| Anhui | East China inland | C2–C3 | 304 | HL / ET | Humidity swing; sealed sample |
| Sichuan | Southwest humid | C2–C3 | 304 | SB / AFP | High humidity; film adhesion |
| Chongqing | Southwest humid | C3 | 304 | PVD / HL | Fog humidity; acid rain |
| Guizhou | Southwest humid | C2–C3 | 304 | HL / EMB | Condensation; rear ventilation |
| Yunnan | Southwest plateau | C2 | 304 | 8K / ET | High UV; QUV re-check |
| Xizang | Southwest plateau | C1 | 304 / 316L | PVD / SB | High UV; diurnal range |
| Shaanxi | Northwest inland | C2 | 304 | HL / ET | Dry atmosphere; thermal movement |
| Gansu | Northwest dry-cold | C1–C2 | 304 / 201 | SB / VR | Wind-blown abrasion; coating wear |
| Qinghai | Northwest plateau | C1 | 304 / 316L | PVD / SB | High UV; low-temperature review |
| Ningxia | Northwest dry-cold | C1–C2 | 304 / 201 | HL / EMB | Thermal range; wind-blown sand |
| Xinjiang | Northwest dry-cold | C1–C2 | 304 / 201 | SB / VR | Extreme range; dry atmosphere |
| Jilin | Northeast severe cold | C2 | 304 | HL / EMB | Freeze–thaw; de-icing salts |
| Heilongjiang | Northeast severe cold | C2 | 304 | HL / SB | Low-temperature movement |
| Hong Kong, China | South China coast | C4 high salt / humidity | 316L | PVD + AFP | Coastal salt; cladding maintenance |
| Macao, China | South China coast | C4 high salt / humidity | 316L | PVD + AFP | Coastal salt; typhoon fixings |
| Taiwan, China | Southeast coast | C4 high salt / humidity | 316L | PVD + AFP | High salt / heat; seismic connections |